portada Superalloy Lattice Block Structures
Type
Physical Book
Publisher
Language
English
Pages
22
Format
Paperback
Dimensions
24.6x18.9x0.1 cm
Weight
0.06 kg.
ISBN13
9781289146191

Superalloy Lattice Block Structures

Nasa Technical Reports Server (Ntrs) (Author) · M. V. Nathal (Author) · Bibliogov · Paperback

Superalloy Lattice Block Structures - Nathal, M. V. ; Nasa Technical Reports Server (Ntrs) ; Et Al

New Book Imported to Netherlands
Delivery: 16 Nov - 23 Nov Shipping: 16 to 20 business days.
€ 21,36
Import costs and 9% BTW included in the price ✅
€ 21,36

Synopsis "Superalloy Lattice Block Structures"

Initial investigations of investment cast superalloy lattice block suggest that this technology will yield a low cost approach to utilize the high temperature strength and environmental resistance of superalloys in lightweight, damage tolerant structural configurations. Work to date has demonstrated that relatively large superalloy lattice block panels can be successfully investment cast from both IN-718 and Mar-M247. These castings exhibited mechanical properties consistent with the strength of the same superalloys measured from more conventional castings. The lattice block structure also accommodates significant deformation without failure, and is defect tolerant in fatigue. The potential of lattice block structures opens new opportunities for the use of superalloys in future generations of aircraft applications that demand strength and environmental resistance at elevated temperatures along with low weight.

Customers reviews

Frequently Asked Questions about the Book

All books in our catalog are Original.
The book is written in English.
The binding of this edition is Paperback.